FIELD: mining.
SUBSTANCE: stowing composition comprising portland cement, plastifying agent, fine-grained filler - sand and water, additionally comprises as a binder the milled tailings of wet magnetic separation of ferrous quartzites with an average particle size of 2.071 microns, as a plastifying agent - superplasticiser SP-1, and the sand with an average particle size of 62.26 microns with the following ratio of components, wt %; the said cement - 13.48; the said sand - 56.43; the said wastes - 2.70; superplasticiser SP-1 - 0.138; water - the rest.
EFFECT: decrease in cement consumption, and increase in the strength of the stowing composition, use of sand with a lower fineness modulus.
1 ex, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
BACKFILLING COMPOSITE MATERIAL | 2014 |
|
RU2568657C1 |
COMPOSITE MATERIAL FOR BACKFILLING OF MINED-OUT SPACE | 2014 |
|
RU2565288C1 |
COMPOSITE BACKFILLING MATERIAL | 2014 |
|
RU2565290C1 |
COMPOSITION OF FILL MIXTURE | 2011 |
|
RU2455493C1 |
HARDENING STOWING MIXTURE | 2011 |
|
RU2456456C1 |
COMPOSITION OF FILLING MASS | 2012 |
|
RU2513897C1 |
FILLING MIXTURE COMPOUND | 2010 |
|
RU2430238C1 |
FILLING MIXTURE COMPOSITION | 2010 |
|
RU2433274C1 |
FILLING MIXTURE COMPOUND | 2010 |
|
RU2425980C1 |
FILLING MIXTURE COMPOUND | 2010 |
|
RU2431044C1 |
Authors
Dates
2014-10-20—Published
2013-04-24—Filed