FIELD: construction.
SUBSTANCE: charge for production of a porous filler contains, wt %: montmorillonite clay 81.0-87.5, dolomite 2.0-3.0, 3% solution of hydrogen peroxide 0.5-1.0, quartz sand 10.0-15.0.
EFFECT: increased strength of a porous filler produced from charge.
1 tbl