FIELD: chemistry.
SUBSTANCE: method includes application of active soda solution, subjected to electrochemical and/or photoelectrochemical processing, and leaching by supply of leaching solution, containing complexants for gold, for its extraction. Hydrogen peroxide is introduced into soda solution after electrochemical processing with obtaining active carbonate-peroxide solution. After that obtained active carbonate-peroxide solution is supplied into gold-containing mineral mass, carbonate-peroxide solution being supplied cyclically, alternating with cycles of supply of leaching solution, until acceptable level of gold extraction is achieved.
EFFECT: increase of process efficiency due to formation of mineral mass of raw material more permeable for leaching solution.
2 cl, 1 dwg, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR HEAP LEACHING OF GOLD FROM MINERAL RAW MATERIAL | 2015 |
|
RU2608481C2 |
METHOD OF LEACHING METALS FROM REFRACTORY CARBONACEOUS ORES (VERSIONS) | 2016 |
|
RU2635582C1 |
METHOD FOR HEAP LEACHING OF GOLD FROM REFRACTORY ORES AND TECHNOGENIC MINERAL RAW MATERIAL | 2015 |
|
RU2585593C1 |
METHOD OF LEACHING GOLD FROM REFRACTORY ORES | 2017 |
|
RU2647961C1 |
METHOD FOR EXTRACTION OF DISPERSE GOLD FROM REFRACTORY ORES AND TECHNOGENIC MINERAL RAW MATERIAL | 2011 |
|
RU2490345C1 |
METHOD FOR HEAP LEACHING OF GOLD FROM REFRACTORY ORES AND TECHNOGENIC MINERAL RAW MATERIAL | 2015 |
|
RU2608479C1 |
METHOD OF DISPERSE GOLD EXTRACTION FROM REFRACTORY ORE AND MAN-MADE MINERAL STOCK | 2013 |
|
RU2509166C1 |
METHOD OF EXTRACTION OF DISPERSE GOLD FROM REFRACTORY ORES OF TECHNOGENIC MINERAL RAW MATERIALS (VERSIONS) | 2014 |
|
RU2566227C1 |
METHOD FOR HEAP LEACHING OF GOLD FROM REFRACTORY ORES | 2014 |
|
RU2580356C1 |
METHOD OF HEAP LEACHING OF DISPERSE GOLD FROM REFRACTORY ORES | 2014 |
|
RU2566231C1 |
Authors
Dates
2015-02-27—Published
2014-03-03—Filed