FIELD: construction.
SUBSTANCE: concrete mix includes, wt %: Portland cement 24.0-26.0; foam glass crumbs of 5-10 mm fraction 54.0-55.5; liquid sodium glass with density of 1500 kg/m3 2.5-3.5; superplasticiser S-3 1.0-1.5; water 15.0-17.0.
EFFECT: reduced heat conductivity.
1 tbl