FIELD: construction.
SUBSTANCE: furnace charge for porous filler production contains, wt %: montmorillonite clay 95.5-97.0, coal 1.0-1.5 ground until passing through the mesh No. 0.63, kaolin 1.0-1.5 sifted through the mesh No. 5, impregnated with saturated water solution of solution sodium borate and wood sawdust 1.0-1.5 dried up to humidity no more than 6%.
EFFECT: increase of strength of the porous filler produced from furnace charge.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
MIXTURE FOR MAKING POROUS AGGREGATE | 2012 |
|
RU2486143C1 |
CHARGE FOR POROUS FILLER PRODUCTION | 2014 |
|
RU2538576C1 |
CHARGE STOCK FOR PRODUCTION OF POROUS AGGREGATE | 2013 |
|
RU2522648C1 |
MIXTURE FOR MAKING POROUS AGGREGATE | 2015 |
|
RU2581169C1 |
CERAMIC MIXTURE FOR MAKING BRICK | 2012 |
|
RU2482090C1 |
MIXURE FOR MAKING POROUS AGGREGATE | 2012 |
|
RU2489378C1 |
CHARGE FOR POROUS FILLER MANUFACTURING | 2013 |
|
RU2525411C1 |
CHARGE FOR POROUS FILLER PRODUCTION | 2014 |
|
RU2561384C1 |
CHARGE FOR MANUFACTURE OF EXPANDED AGGREGATE | 2016 |
|
RU2610004C1 |
MIXTURE FOR MAKING POROUS AGGREGATE | 2012 |
|
RU2486148C1 |
Authors
Dates
2015-09-10—Published
2014-10-21—Filed