FIELD: metallurgy.
SUBSTANCE: granulated aluminium containing the deoxidant is supplied into the fusion flow by pulsing high-speed flow of carrier gas at the frequency 5-15 Hz, and the angle between conditional axes of the flow of steel and the flow of granules of aluminium is maintained within 15-30 degrees. During supply variation of angle of flow of granules amounts 2-4 degrees.
EFFECT: invention allows to optimise conditions of adding of granules as far as the flow of aluminium granules is completely absorbed by metal flow without recoiling and a passing the flow through, with aluminium waste decrease.
3 cl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR REDUCING OF STEEL IN LADLE | 2005 |
|
RU2286393C1 |
METHOD OF DEOXIDIZING AND ALLOYING STEEL IN LADLE | 0 |
|
SU1154341A1 |
MANUFACTURING METHOD OF LOW-SILICON STEEL | 2008 |
|
RU2353667C1 |
ACTIVE DEOXIDIZER OF LIQUID AND REFRACTORY HOT AND COLD SLAGS | 2022 |
|
RU2786789C1 |
LOW-SILICON STEEL PRODUCTION METHOD | 2023 |
|
RU2818526C1 |
METHOD OF TREATMENT OF STEEL IN LADLE | 2001 |
|
RU2185448C1 |
METHOD FOR SMELTING STEEL FOR AUTOMATIVE-USE SHEET | 0 |
|
SU981385A1 |
PROCESS FOR STEEL PRODUCTION | 0 |
|
SU908843A1 |
METHOD OF STEEL PRODUCTION | 0 |
|
SU817073A1 |
METHOD OF MOLTEN STEEL ALLOYING WITH ALUMINIUM | 0 |
|
SU765373A1 |
Authors
Dates
2015-09-10—Published
2014-07-11—Filed