FIELD: chemistry.
SUBSTANCE: mixture for making foamed glass contains, wt %: ground scrap glass - 75.0-90.0; thermal power plant water treatment wastes - 10.0-25.0. The wastes have the following components, wt %: iron hydroxide 5.0-10.0; calcium and magnesium hydroxides 2.0-4.0; gypsum - 2.0-5.0; calcium carbonate - the balance.
EFFECT: wider raw material base for making foamed glass.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
MIXTURE FOR MAKING FOAMED GLASS | 2011 |
|
RU2487842C1 |
CHARGE FOR POROUS FILLER PRODUCTION | 2014 |
|
RU2561387C1 |
RAW MIXTURE USED FOR MANUFACTURING FOAM GLASS | 2008 |
|
RU2369571C1 |
MIXTURE FOR MAKING POROUS AGGREGATE | 2012 |
|
RU2496732C1 |
RAW MIXTURE FOR MAKING FOAMED GLASS | 2009 |
|
RU2411200C1 |
RAW MIX FOR PRODUCTION FOAM GLASS | 2007 |
|
RU2358927C1 |
RAW MATERIAL MIX FOR CELLULAR GLASS PRODUCTION | 2006 |
|
RU2335474C2 |
FOAMGLASS | 2006 |
|
RU2325361C1 |
CHARGE FOR PRODUCTION OF POROUS FILLER | 2012 |
|
RU2505497C1 |
METHOD OF FOAMED GLASS PRODUCTION | 2011 |
|
RU2502686C2 |
Authors
Dates
2015-09-20—Published
2014-10-21—Filed