FIELD: chemistry.
SUBSTANCE: invention relates to deicing materials based on alimentary cooking salt, calcined calcium chloride, corrosion inhibitors, and can be used for obtaining solid deicing material with low corrosion activity. A method for producing a solid deicing material comprises a mechanical uniform mixing between a crystal of common salt stone Class I crystalline calcium chloride calcined first technical grade crystalline metal corrosion inhibitor elements, crystalline surfactant crystalline acidity regulator. During production of deicing material each element of corrosion inhibitor is saturated with heavy isotopes of carbon 13C so that ratio of carbon isotopes 13C to total amount of carbon in element makes from 0.005 to 0.75, and each element of corrosion inhibitor is saturated with heavy isotopes of nitrogen 15N so that ratio of nitrogen isotopes 15N to total amount of nitrogen in element makes from 0.0001 to 0.1375.
EFFECT: higher efficiency of corrosion inhibitor in obtained solid deicing material due to enrichment of corrosion inhibitor heavy isotopes carbon 13C and nitrogen 15N in reactor plant with cavitation reactor.
5 cl, 4 dwg, 69 tbl
Authors
Dates
2016-12-10—Published
2015-03-04—Filed