FIELD: construction.
SUBSTANCE: composition for the porous aggregate production includes, wt %: liquid sodium glass with the density of 1.41 g/cm3 50-75, sodium chloride ground to the size less than 0.3 mm, 1-3, burnt rocks ground before passing through the 0.14 mm sieve, 12-34, microsilica from the ferrosilicon and ferroalloys production with the average particle size of not more than 0.25 microns and containing oxides, wt %: SiO2 97.8; CaO 1.3; MgO 0.4; R2O 0.5, 10-15.
EFFECT: increasing the compressive strength and the softening coefficient of the porous aggregate, industrial waste recycling.
3 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION FOR MAKING POROUS AGGREGATE | 2015 |
|
RU2594238C1 |
COMPOSITION FOR POROUS AGGREGATE PRODUCTION | 2016 |
|
RU2618244C1 |
COMPOSITION FOR MAKING POROUS AGGREGATE | 2015 |
|
RU2589120C1 |
COMPOSITION FOR MANUFACTURE OF EXPANDED AGGREGATE | 2016 |
|
RU2614339C1 |
COMPOSITION FOR PRODUCING POROUS AGGREGATE | 2016 |
|
RU2615557C1 |
COMPOSITION FOR PRODUCING WATER-RESISTANT POROUS AGGREGATE | 2011 |
|
RU2481286C2 |
CERAMIC COMPOSITION FOR MANUFACTURING WALL MATERIALS | 2015 |
|
RU2613702C1 |
COMPOSITION FOR MAKING POROUS AGGREGATE | 2017 |
|
RU2649206C1 |
COMPOSITION FOR PRODUCTION OF POROUS AGGREGATE | 2014 |
|
RU2555171C1 |
COMPOSITION FOR PRODUCTION OF POROUS FILLER | 2014 |
|
RU2575659C1 |
Authors
Dates
2017-06-09—Published
2016-04-27—Filed