FIELD: soil reclamation.
SUBSTANCE: invention relates to composition of the material for thermal soil reclamation. The proposed material contains a mineral component. The feature of the proposed material is that it contains ground serpentine as a mineral component. It additionally contains ground brown coal. The ratio of brown coal: serpentine by weight is from 1.7 to 3.3. The rational size of particles of the material components is no more than 4 mm.
EFFECT: increased thermal reclamation characteristics of the material due to the change of its interaction with solar radiation, as well as providing aggregate properties close to natural black earth with simultaneous solving the problem of using only natural components.
2 cl