FIELD: enrichment of minerals.
SUBSTANCE: proposed invention can be used in processing of mineral raw material containing pyrrhotite. Method for concentration of sulphide pyrrhotite-containing ores includes main, recleaning operations in a cycle of collective copper-zinc flotation, main, control, two cleaning operations in copper flotation cycle. In addition, a zinc flotation cycle is carried out, which includes the main, control and one recleaning operations. In copper flotation cycle one additional recleaning flotation operation is performed. Hydrogen peroxide is added to the collective recleaning operation of flotation, to the first and second recleaning operations of copper flotation, to the main zinc flotation and to recleaning zinc flotation. Hydrogen peroxide is added to collective cleaner flotation in amount of 200–300 g/t of initial ore. In the first cleaning copper flotation and in the cleaning zinc flotation hydrogen peroxide is added in amount of 50 to 100 g/t of initial ore. In the second cleaning copper flotation hydrogen peroxide is introduced in amount of 50 to 150 g/t of initial ore. Hydrogen peroxide is added to the main zinc flotation in amount of 100 to 150 g/t of initial ore.
EFFECT: increased efficiency of flotation concentration of sulphide copper-zinc pyrrhotite-containing ores, increased rate of flotation of copper and zinc minerals, increased level of copper and zinc extraction into concentrates of the same name.
1 cl, 4 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PYRRHOTITE-BEARING ORES FLOTATION | 2011 |
|
RU2475308C1 |
METHOD FOR ENRICHMENT POLYMETALLIC ORES CONTAINING NICKEL, COPPER AND IRON SULFIDE MINERALS | 2015 |
|
RU2613687C1 |
METHOD OF SELECTIVE SEPARATION OF PENTLANDITE AGAINST IRON-BEARING MATERIALS AT CONCENTRATION OF SOLID SULFIDE HIGH COPPER-NICKEL GRADES | 2008 |
|
RU2372145C1 |
METHOD FOR FLOTATION SEPARATION OF SULFIDE COPPER-NICKEL PYRRHOTINE-BEARING ORES | 2006 |
|
RU2320423C2 |
PROCEDURE FOR PROCESSING ANTIMONY-ARSENIC SULPHIDE GOLD CONTAINING ORE | 2010 |
|
RU2432407C1 |
METHOD FOR FLOTATION CONCENTRATION OF SULFIDE COPPER-NICKEL ORES | 2009 |
|
RU2397817C1 |
METHOD OF FLOTATION ENRICHMENT OF SULPHIDIC COPPER-NICKEL ORES | 2009 |
|
RU2398636C1 |
MODIFIED REAGENT FOR FLOTATION OF NONFERROUS METAL ZINC-BEARING ORES | 2012 |
|
RU2496583C1 |
METHOD OF DRESSING OF SULPHIDIC COPPER-NICKEL PIRRHOTINE-CONTAINING ORES | 2005 |
|
RU2291747C1 |
METHOD OF FLOTATION ENRICHMENT OF SULPHIDIC COPPER-NICKEL ORES | 2009 |
|
RU2404858C1 |
Authors
Dates
2024-06-25—Published
2023-09-04—Filed