FIELD: chemical-thermic working. SUBSTANCE: composition has the following components, wt.-% tin bronze БP 0-10 40-60; amorphous boron 8-12; zinc 2-4; aluminium oxide 2-3; potassium tetrafluoroborate 1-3, and boron carbide the rest. Use of proposed composition ensures to increase corrosion resistance of steel articles by 2-3 times and intensify saturation process by 5-6 times. EFFECT: intensified process, increased corrosion stability. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION FOR COMPLEX SATURATION OF STEEL PARTS | 1986 |
|
SU1356527A1 |
METHOD AND COMPOUND FOR BORATING OF STEEL ARTICLES | 1987 |
|
SU1452182A1 |
COMPOSITION FOR DIFFUSION BORONIZING OF METAL PRODUCTS | 0 |
|
SU943321A1 |
METHOD OF BORATING STEEL ARTICLES | 0 |
|
SU1578227A1 |
COMPOSITION FOR COMPLEX SATURATION OF STEEL ARTICLES | 1987 |
|
SU1438269A1 |
COMPOSITION FOR BORATING STEEL ARTICLES | 0 |
|
SU1571102A1 |
BORON-ALUMINIZING METHOD OF STEEL SURFACE | 2018 |
|
RU2691431C1 |
METHOD OF BORIDING-CHROMIZING OF STEEL PRODUCTS | 0 |
|
SU1659528A1 |
METHOD FOR COMPLEX CASEHARDENING OF STEEL PRODUCTS | 0 |
|
SU973667A1 |
BORONIZING COMPOSITION | 0 |
|
SU765398A1 |
Authors
Dates
1995-12-10—Published
1986-03-27—Filed