FIELD: mechanical engineering. SUBSTANCE: method includes the steps of cast-iron liner aluminizing and aluminium ribbed jacket casting- in, with cast-iron liner external surface aluminizing effected through metallization. The finished ribbed cylinder is thermally treated at 570 ± 10 C for 5 to 10 hours depending on the wall thickness. The method enables the aluminizing time to be substantially reduced (from 15-20 min to 1 min) with high degree of adhesion of cast iron and aluminium layers. EFFECT: reduced time of treatment. 4 dwg
Title | Year | Author | Number |
---|---|---|---|
PRESS-MOLD FOR MAKING BIMETALLIC CYLINDERS | 1992 |
|
RU2038917C1 |
CORE FOR CASTING FINNED CYLINDER OF ENGINES | 0 |
|
SU1088864A1 |
BIMETAL CYLINDER OF AIR-COOLED INTERNAL COMBUSTION ENGINE | 0 |
|
SU1686205A1 |
CASTING OF INTERNAL COMBUSTION ENGINE CYLINDER BLOCK AND METHOD FOR MAKING IT | 1998 |
|
RU2146183C1 |
CASTING MOULD PRODUCTION METHOD | 0 |
|
SU831351A1 |
METHOD AND DEVICE FOR CASTING IN MOULD | 2013 |
|
RU2541267C2 |
METALLIZING DEVICE | 0 |
|
SU885338A1 |
COMPONENT FOR CASTING WITH USAGE OF EMBEDDED PARTS, CYLINDER SLEEVE, BLOCK OF CYLINDERS AND MANUFACTURING METHOD OF CYLINDER SLEEVE | 2006 |
|
RU2376107C2 |
CYLINDER SLEEVE AND METHOD OF ITS MANUFACTURE | 2013 |
|
RU2627526C2 |
BIMETAL CASTING METHOD | 0 |
|
SU789227A1 |
Authors
Dates
1994-01-30—Published
1992-09-07—Filed