FIELD: luminescence dying of polyethylene. SUBSTANCE: concentrate contains high pressure polyethylene ( 53.37-58.37% ), liquid paraffin for producing protein-vitamin concentrate (4.73-10.24% ), fluorescence pigment ( 34.58-36.45% ) and absorber of formaldehyde-ammonia salt (0.69-2.28% ). Mentioned above pigment is prepared on the base of melamine-toluene-sulfamide-formaldehyde or melamine-areatoluene-sulfamide-formaldehyde polymer and luminescence component. Method of producing concentrate involves feeding into mixer granulated high pressure polyethylene and fluorescence pigment as pieces 2-120 mm in size and mixing at ambient temperature till particles of pigment are 0.5-1.0 mm in size. Into thus prepared mass liquid paraffin is added and mixture is ground within 0.5-2 h. Then absorber of formaldehyde is added by heating and grinding is carried out at 120-145 C within 1.5-2.5 h. EFFECT: improves desired product quality. 3 cl, 5 tbl
Title | Year | Author | Number |
---|---|---|---|
LUMINESCENT COLORED POLYETHYLENE COMPOSITION | 1982 |
|
SU1086766A1 |
4-CARBOXYMETHYLAMINONAPHTHALIC ACID N-CARBOXYMETHYLIMIDE AS A GREEN LUMINOSITY LUMINOPHORE, AND A METHOD OF ITS PREPARING | 0 |
|
SU1816787A1 |
COMPOSITION FOR PREPARING DIENE FLUORORESCENT PIGMENTS | 1987 |
|
SU1642742A3 |
DAY FLUORESCENT PIGMENT | 0 |
|
SU671351A1 |
METHOD OF PRODUCING DAY FLUORESCENT PIGMENTS | 0 |
|
SU1174448A1 |
COMPOSITION FOR PRODUCTION OF FLUORESCENT LIGHTING PIGMENT FOR POLYETHYLENE DYEING | 0 |
|
SU1420937A1 |
POLYMERIC COMPOSITION | 1999 |
|
RU2163915C2 |
PLASTIC SCINTILLATOR | 1991 |
|
RU2012904C1 |
COLORING POLYMERIC COMPOSITION CONCENTRATE | 1997 |
|
RU2129136C1 |
METHOD OF PRODUCING MATERIAL FOR PRODUCING LIGHT-CORRECTING POLYMER FILM | 2013 |
|
RU2567909C2 |
Authors
Dates
1994-02-15—Published
1991-03-29—Filed