FIELD: building materials. SUBSTANCE: binder has, mas. p. : novolacs phenolformaldehyde oligomer 100; hexamethylenetetramine 6-12; waste after silicon oxide reduction 5-15. Powder-like novolac resin and hexamethylene are stirred for 30 min, then finely dispersed silicon oxide is added and stirred for 30 min. Binder properties: crushing strength is 85-98 MPa, crushing strength after thermal loading at 300 C for 30 min is 57-69 MPa. EFFECT: enhanced quality of binder. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
POWDERY POLYMER COMPOSITION FOR PRODUCTION OF ABRASIVE INSTRUMENT | 1992 |
|
RU2057151C1 |
ABRASIVE PASTE | 1993 |
|
RU2047475C1 |
MASS FOR MANUFACTURING ABRASIVE TOOL | 0 |
|
SU1743827A1 |
ABRASIVE MASS | 0 |
|
SU1077770A2 |
BINDING AGENT | 2002 |
|
RU2216556C1 |
METHOD FOR MANUFACTURING ABRASIVE TOOL | 1990 |
|
RU2009866C1 |
MASS FOR MAKING AN ABRASIVE TOOL | 0 |
|
SU960000A1 |
METHOD OF PRODUCING ABRASIVE TOOL | 0 |
|
SU1611719A1 |
COMPOUND FOR MANUFACTURING ABRASIVE TOOLS | 0 |
|
SU1380924A1 |
METHOD OF MANUFACTURING ABRASIVE TOOL | 0 |
|
SU1088921A1 |
Authors
Dates
1994-04-15—Published
1990-06-21—Filed