FIELD: preparing ores and concentrates for melting. SUBSTANCE: during caking concentrate is mixed with complex binder. Said binder contains oil wastes and liquid glass at ratio 0.5: 1, expense being 20 mass % of concentrate. Calcination is carried out at 300-350 C. EFFECT: decreases calcination temperature, decreases energy expense, increases strength of fluorospar briquettes. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCING PELLETS OF FLUORSPAR | 0 |
|
SU910814A1 |
METHOD FOR PRODUCING PELLETS OF FLUORSPAR | 0 |
|
SU979512A1 |
METHOD FOR PREPARING LIQUID-SLUDGE BURDEN FOR BRIQUETTING | 1991 |
|
SU1822584A3 |
METHOD OF BRIQUETTING FLOATATION FLUORITE CONCENTRATES | 2004 |
|
RU2268314C1 |
METHOD OF IRON-ORE BENEFICATION | 0 |
|
SU1488012A1 |
METHOD OF PRECIPITATION OF SOLID SUSPENSIONS IN REUSED WATER IN COAL FLOTATION | 1993 |
|
RU2019258C1 |
METHOD FOR PRODUCING FLUORSPAR BRIQUETTES | 2002 |
|
RU2205235C1 |
METHOD FOR CLARIFYING SUSPENSIONS FROM GAS CLEARING IN ALUMINIUM PRODUCTION | 1993 |
|
RU2036164C1 |
METHOD OF SOLUTION CLEARING OFF SULFATES | 1991 |
|
RU2033395C1 |
METHOD FOR PRECIPITATING SOLID SUSPENSION FROM SUSPENSION AFTER GAS CLEANING ALUMINIUM PRODUCTION | 0 |
|
SU1834676A3 |
Authors
Dates
1994-04-30—Published
1990-09-18—Filed