FIELD: production of building materials. SUBSTANCE: in the method of manufacture of stone-cast products by preparation of melt and casting of it in moulds in the initial stage the melt is prepared from a semiconductor element placed between electrodes, and ash heated to 450 to 550 C is delivered to the melt place by several flows until the preset space of the furnace is filled with fused ash, then ash is delivered at a rate providing the presence of the ash solid phase in the melt at casting in moulds up to 25 to 30 percent by mass. The semiconductor element consists of ash - 25 to 30 percent by mass, clay - 45 to 60 percent by mass, iron or graphite - 10 to 60 percent by mass. EFFECT: facilitated procedure. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MANUFACTURE OF PIG IRON GRINDING BODIES | 1992 |
|
RU2016077C1 |
METHOD OF DETERMINING CHANGES IN COEFFICIENT OF SURFACE TENSION AT SOLID BODY/LIQUID BOUNDARY | 1991 |
|
RU2053496C1 |
METHOD OF PRODUCING ARTICLES FROM MOLTEN MATERIAL | 0 |
|
SU1544573A1 |
WEAR RESISTANT COLD-RESISTANT STEEL | 1995 |
|
RU2087581C1 |
MOULDABLE STONE COMPOSITION | 0 |
|
SU1382830A1 |
METHOD OF OBTAINING STONE CASTING | 0 |
|
SU1735004A1 |
METHOD FOR STONE CASTING PRODUCTION | 0 |
|
SU1790490A3 |
0 |
|
SU270574A1 | |
FLUOROFLOGOPITE-BASED MICA CRYSTAL MATERIAL AND METHOD OF ITS PRODUCTION | 2014 |
|
RU2559964C1 |
METHOD FOR PREPARATION ARTICLES OF SILICATE MELTS | 0 |
|
SU1738659A1 |
Authors
Dates
1994-05-15—Published
1991-10-31—Filed