FIELD: oil and gas producing industry. SUBSTANCE: oil-well cement contains (in % by mass): portland cement 7-14, sulfo compound 6-13, sulfo aluminate hydraulic binder 73-87. The sulfo aluminate hydraulic binder has the following phase composition (in % by mass): calcium sulfo aluminate 10-30, double-calcium silicate 67-75, double-calcium ferrite 3-10. As sulfo compound may be used gypsum dihydrate, or phosphogypsum, or boron gypsum. EFFECT: improved properties. 2 cl, 1 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| EXPANDABLE OIL-WELL CEMENT | 1997 | 
 | RU2153059C2 | 
| OIL WELL CEMENT FOR LOW-TEMPERATURE WELLS | 1997 | 
 | RU2144977C1 | 
| LIGHT-WEIGHT GROUTING COMPOSITION FOR WELL CEMENTING IN HIGH-PERMEABILITY ROCKS UNDER CONDITIONS OF HYDROGEN SULPHIDE AGGRESSION | 2016 | 
 | RU2741890C2 | 
| EXPANDING PLUGGING COMPOSITION FOR LOW-TEMPERATURE WELLS | 1998 | 
 | RU2155263C2 | 
| GROUTING COMPOSITION | 2001 | 
 | RU2202033C2 | 
| EXPANDABLE BRIDGING MATERIAL | 0 | 
 | SU1808995A1 | 
| GYPSUM-CEMENT PLUGGING MIXTURE | 1996 | 
 | RU2127798C1 | 
| EXPANDABLE GROUTING MATERIAL | 1996 | 
 | RU2111341C1 | 
| METHOD FOR PRODUCING CEMENT CLINKER IN ROTARY KILN | 0 | 
 | SU1039913A1 | 
| PLUGGING MATERIAL FOR HIGH-TEMPERATURE WELLS | 2000 | 
 | RU2198999C2 | 
Authors
Dates
1994-05-30—Published
1991-03-18—Filed