FIELD: oil and gas producing industry. SUBSTANCE: plugging composition contains (parts by mass): portland cement 80-120; fly ash 80-120; asbestos 2-3; a mineral salt 1.0-1.5; and water 120. As the mineral salt is used a mixture of sodium chloride and sulfate, with chloride to sulfate ratio of 1: 1. The plugging composition features good deforming properties, increased strength of cement stone, and increased adhesion of cement stone with casing string. EFFECT: improved properties. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
LIGHT GROUTING COMPOUND | 1991 |
|
RU2021488C1 |
GROUTING COMPOUND | 1991 |
|
RU2030556C1 |
OIL WELL CEMENT FOR LOW-TEMPERATURE WELLS | 1997 |
|
RU2144977C1 |
METHOD OF GROUTING MORTAR-PREPARATION | 2002 |
|
RU2213844C1 |
LIGHT-WEIGHT GROUTING MIXTURE | 2016 |
|
RU2642897C1 |
DRY MIXTURE FOR PREPARING EXPANDING GROUTING MORTAR | 2019 |
|
RU2710943C1 |
COMPLEX ADDITIVE TO GROUTING MORTAR BASED ON PORTLAND CEMENT | 1994 |
|
RU2078908C1 |
EXPANDING PLUGGING COMPOSITION FOR LOW-TEMPERATURE WELLS | 1998 |
|
RU2155263C2 |
METHOD OF WELLS CASING AND CEMENTING | 1992 |
|
RU2068489C1 |
GROUTING MORTAR FOR REPAIR JOBS AND WELL LINING | 1992 |
|
RU2035585C1 |
Authors
Dates
1994-05-30—Published
1991-07-22—Filed