FIELD: making stemming of blastholes. SUBSTANCE: hardening mixture contains the following components, mass %: dolomite dust 25.7-27.5; lignosulfonate 4.8-8.5; water 11.4-13.8; potassium alum 9.5-11.5; the balance natural anhydrite, fraction of 0.4-1.0 mm. EFFECT: higher efficiency and safety in mining. 6 tbl, 2 dwg
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION OF SOLIDIFYING MIXTURE | 1992 |
|
RU2047777C1 |
COMPOSITION OF SOLIDIFYING MIXTURE | 0 |
|
SU1580027A1 |
COMPOSITION FOR PREPARING STEMMING MATERIAL FOR INSULATING EXPLOSIVE CHARGE | 2023 |
|
RU2832474C1 |
COMPOSITION OF FILLING MIXTURE | 2023 |
|
RU2824526C1 |
COMPOSITION OF QUICK-SETTING MIX | 0 |
|
SU619681A1 |
STOWING MIXTURE AND METHOD OF PRODUCTION OF THIS MIXTURE | 0 |
|
SU1773278A3 |
METHOD FOR PREPARING ANHYDRIDE BINDING AGENT | 2002 |
|
RU2277515C2 |
METHOD FOR MANUFACTURE OF PRODUCTS FROM ANHYDRITE | 2007 |
|
RU2356866C1 |
COMPOSITION FOR REFILLING SPACE BEHIND SUPPORT OF MINE WORKING | 0 |
|
SU1571264A1 |
METHOD OF PREPARATION OF CAST HARDENING INSERTION IN BALL MILL | 1990 |
|
RU2013131C1 |
Authors
Dates
1994-08-30—Published
1992-06-30—Filed