FIELD: chemical industry. SUBSTANCE: in manufacturing a composite material, carbamidoformaldehyde resin (CFR) is added to the compound prior to the addition of a coagulant. CFR having a gelatinization time of 140-260 s is used in the form of a dispersion which represents a product of suspension polycondensation of carbamide and formaldehyde in the presence of a protective colloid such as a copolymer of butylacrylate, butylmethacrylate and methacrylic acid, their weight ratio being 1:(0.41-0.45):(0.15-0.19) and the carbamide to protective colloid ratio being 1:(0.05-0.12). EFFECT: improved properties of the composite material. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURING PAPER FOR INNER LAYERS OF DECORATIVE LAMINATE-PAPER PLASTIC | 0 |
|
SU1786214A1 |
METHOD OF MANUFACTURING PHENOL-FORMALDEHYDE RESIN DISPERSION | 1991 |
|
RU2035471C1 |
METHOD FOR PRODUCTION OF PAPER FOR INNER LAYERS OF DECORATIVE PLASTIC LAMINATE | 0 |
|
SU1677132A1 |
METHOD OF PRODUCING PAPER FOR INNER LAYERS OF DECORATIVE LAMINATED PAPER PLASTIC | 0 |
|
SU1756445A1 |
METHOD OF PRODUCING PAPER FOR INNER LAYERS OF DECORATIVE PAPER-PLASTIC LAMINATE | 0 |
|
SU1425262A1 |
METHOD OF MANUFACTURING PAPER MATERIAL FOR INTERNAL LAYER OF DECORATIVE PAPER-LAYERED PLASTIC | 1996 |
|
RU2096549C1 |
METHOD OF PRODUCING DECORATIVE BACKING PAPER | 0 |
|
SU1481307A1 |
PAPER-PLASTIC WEB LAMINATE | 0 |
|
SU1490209A1 |
METHOD OF MAKING DECOPATIVE PAPER-PLASTIC LAMINATE | 0 |
|
SU889770A1 |
PROCESS FOR THE MANUFACTURE OF PAPER AND CARDBOARD FOR LAMINATED PLASTICS | 0 |
|
SU681141A1 |
Authors
Dates
1994-09-15—Published
1992-01-13—Filed