FIELD: building materials. SUBSTANCE: raw mixture for claydite producing has, wt.-%: clay raw 97-98; waste of electroplating manufacture containing cobalt oxide 1.3-2 and flax dust 0.7-1. Claydite properties: roasting temperature is 1140 C, granule density is 0,47-0,50 g/cm3, swelling coefficient is 3.4-3.8. EFFECT: enhanced quality of claydite. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
CRUDE MIXTURE FOR MAKING EXPANDED CLAY | 2010 |
|
RU2463269C2 |
MIXTURE FOR PRODUCING EXPANDED CLAY AGGREGATE | 0 |
|
SU1715751A1 |
METHOD FOR CLAYDITE PRODUCTION | 1992 |
|
RU2031880C1 |
STARTING MATERIAL FOR CLAYDITE | 1998 |
|
RU2134671C1 |
METHOD OF CLAYDITE PREPARING | 1992 |
|
RU2031879C1 |
RAW MIXTURE FOR PRODUCING EXPANDED CLAY AGGREGATE | 0 |
|
SU1636371A1 |
METHOD FOR PRODUCTION OF EXPANDED CLAY AGGREGATE | 1991 |
|
RU2045490C1 |
RAW MATERIALS MIXTURE FOR PRODUCTION OF CLAYDITE | 1996 |
|
RU2109704C1 |
RAW MATERIAL MIX FOR PRODUCTION OF EXPANDED CLAY AGGREGATE | 1992 |
|
RU2040499C1 |
MIXTURE FOR PRODUCING EXPANDED CLAY AGGREGATE | 0 |
|
SU1715750A1 |
Authors
Dates
1994-11-30—Published
1991-06-24—Filed