FIELD: claydite production. SUBSTANCE: method involves addition of corrective additive - herbicide diphenylamide at concentration 0.5-2 wt.-% (as active substance) to the clay raw following by granulation, drying and calcination of granules following by cooling. Claydite properties: filled mass after addition of 1 wt.-% additive is 380 kg/m3, compression strength at 2.15 MPa in the presence of 2 wt.-% additive is 335 kg/m3 and 1.8 MPa, respectively. EFFECT: improved method of claydite preparing. 1 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| METHOD FOR CLAYDITE PRODUCTION | 1992 | 
 | RU2031880C1 | 
| CRUDE MIXTURE FOR PRODUCING HAYDITE | 1997 | 
 | RU2123481C1 | 
| RAW MIX FOR MANUFACTURING HAYDITE | 1995 | 
 | RU2098374C1 | 
| RAW MIX FOR PREPARING EXPANDES CLAY AGGREGATE | 1999 | 
 | RU2171236C1 | 
| STARTING MATERIAL FOR CLAYDITE | 1998 | 
 | RU2134671C1 | 
| RAW MATERIALS MIXTURE FOR PRODUCTION OF CLAYDITE | 1996 | 
 | RU2109704C1 | 
| RAW MATERIAL MIX FOR PRODUCTION OF EXPANDED CLAY AGGREGATE | 1992 | 
 | RU2040499C1 | 
| RAW MATERIAL MIXTURE FOR PRODUCTION OF EXPANDED CLAY AGGREGATE | 2012 | 
 | RU2520593C2 | 
| RAW MIXTURE FOR CLAYDITE PRODUCING | 1991 | 
 | RU2023700C1 | 
| METHOD FOR PRODUCTION OF EXPANDED CLAY AGGREGATE | 1991 | 
 | RU2045490C1 | 
Authors
Dates
1995-03-27—Published
1992-06-24—Filed