FIELD: steel working. SUBSTANCE: hardened medium has, wt.-%: calcium nitrate 20-48; calcium hydroxide 0.01-0.15, and water - the rest. Use of proposed medium ensures to prevent corrosion of hardening metal and provide its high hardness. EFFECT: enhanced quality of medium. 2 tbl