FIELD: electrochemical polishing. SUBSTANCE: process of electrochemical polishing is carried out in phosphate solution with addition of organic substances at the following ratio of components, wt.-%: o-phosphoric acid (density is 1.73 at 15 C) 60-80; n-butylamine 0.1-1.0; phenetidine chloride 0.3-0.8, and water - the rest. EFFECT: enhanced quality of solution.
Title | Year | Author | Number |
---|---|---|---|
SOLUTION FOR ELECTROCHEMICAL POLISHING OF ZINC | 0 |
|
SU662572A1 |
SOLUTION FOR ELECTROCHEMICAL POLISHING OF BERYLLIUM BRONZE | 0 |
|
SU777087A1 |
SOLUTION FOR ELECTROCHEMICAL POLISHING OF COPPER-ZING-NICKEL ALLOY (GERMAN SILVER) | 0 |
|
SU633889A1 |
SOLUTION FOR ELECTROCHEMICAL POLISHING OF METALLIC SURFACE | 0 |
|
SU692851A1 |
0 |
|
SU550415A1 | |
0 |
|
SU463743A1 | |
METHOD OF PRODUCING LEAD HYDROXIDE | 1991 |
|
RU2006525C1 |
METHOD OF OXYGEN AND HYDROGEN PRODUCTION | 1990 |
|
RU2032769C1 |
ELECTROLYTE FOR SETTLING COATING FROM HIGH-MELTING METALS AND METHOD OF OBTAINING SAME | 1982 |
|
SU1123321A1 |
0 |
|
SU483458A1 |
Authors
Dates
1995-01-20—Published
1991-05-22—Filed