FIELD: metallurgy. SUBSTANCE: speiss is smelted at temperature of 1000-1100 C and atmospheric pressure. Then pyrite is added to the bottom of the smelt bath in amount of 100-150% from the speiss weight. Pyrite is held on the bath bottom by means of bell up to complete interaction of pyrite with speiss components. EFFECT: enhanced efficiency speiss processing. 1 cl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PROCESSING POLYMETALLIC MELTS | 0 |
|
SU973647A1 |
METHOD FOR PROCESSING COPPER-ARSENIC ORES | 0 |
|
SU1054436A1 |
METHOD FOR PROCESSING ARSENIC-CONTAINING DUST OF NON-FERROUS METALLURGY | 2022 |
|
RU2785796C1 |
METHOD OF RECOVERY OF NON-FERROUS METALS FROM COPPER-AND-LEAD WASTES CONTAINING TIN AND ANTIMONY | 1999 |
|
RU2154682C1 |
0 |
|
SU406924A1 | |
METHOD OF GALLIUM-ARSENIC-BEARING WASTES PROCESSING | 1995 |
|
RU2078842C1 |
METHOD OF TREATMENT HARD GOLD-ARSENICAL ORES AND CONCENTRATES AND FURNACE FOR ITS IMPLEMENTATION | 2007 |
|
RU2348713C1 |
TIN-CONTAINING MATERIAL PROCESSING METHOD | 2011 |
|
RU2469114C1 |
METHOD FOR PROCESSING COPPER SLIPS | 0 |
|
SU1100327A1 |
METHOD FOR CONVERTING LEAD-CONTAINING COPPER MATTES | 0 |
|
SU947211A1 |
Authors
Dates
1995-01-27—Published
1992-01-30—Filed