FIELD: building materials. SUBSTANCE: binder has, wt.-% (as dry matter): high calcium ash-flash 30-69; aqueous suspension of kaolinite clay and calcium chloride taken at the ratio (13-30):1 31-70. Compression strength of specimens after 28 days is 16.6-20.2 MPa, water resistance coefficient is 0.61-0.72. EFFECT: enhanced quality of binder. 1 tbl