FIELD: wood working; production of wood particle and fiber boards by dry method. SUBSTANCE: wood particles are prepared and dried by traditional method up to moisture content of 3-5%. Leather particles are used with moisture content of 3-17%. Dried wooden particles are mixed with formaldehyde-containing resin, e. g., KF-MT 15 in the amount of 12% of mass of absolutely dry wooden particles. Introduced by mixing into produced mixture is chrome-tanned leather particles in the amount of 25-60% of the molding material. Mixture is mixed for 4-6 min, and formed into mat and subjected to hot molding at temperature of 140-180 C for 0.3-0.5 min/mm of board at pressure of 2-2.5 MPa. Produced boards are held for 72 h at room temperature, cut into samples and tested. EFFECT: higher efficiency. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF LINING WOOD-FIBER TILES WITH INCRUSTATION COVERING | 1995 |
|
RU2120373C1 |
METHOD FOR PRODUCTION OF WOOD PARTICLE BOARDS | 1992 |
|
RU2074090C1 |
0 |
|
SU1780522A3 | |
METHOD OF MANUFACTURING WOOD PARTICLE BOARD | 0 |
|
SU1521598A1 |
METHOD OF MANUFACTURING WOOD PARTICLE BOARDS | 0 |
|
SU1142291A1 |
METHOD FOR MANUFACTURE OF WOOD PARTICLE BOARDS | 2000 |
|
RU2176186C1 |
METHOD FOR MANUFACTURE OF WOOD-SHAVING BOARDS | 2003 |
|
RU2237574C1 |
PARTICLE BOARD MANUFACTURING PROCESS | 0 |
|
SU1184684A1 |
METHOD OF MANUFACTURING FIBER BOARDS | 0 |
|
SU1371921A1 |
WOOD FIBRE PLATES NON-STOP PRODUCTION METHOD | 0 |
|
SU1691104A1 |
Authors
Dates
1995-04-10—Published
1992-03-17—Filed