FIELD: welding materials. SUBSTANCE: electrode coating contains the following element in mass percentage: ilmenite rock - 26 to 36, marble - 11 to 15, ferromanganese - 15 to 20, ferrotitanium - 5 to 10, quartz sand 20 to 30, kaoline - 6 to 10, wood flour 1.5 to 2.0, soda ash 0.5 to 1.5. Wood flour shall be taken in the ratio 1:(4.0 to 5.0):(7.0 to 7.5). Ilmenite rock used in the coating composition is from the Aldan region and contains 8 to 15% of titanium oxide. Use of this electrode coating ensures mechanical properties of weld seam corresponding to seam type Э46. EFFECT: possibility of use for welding critical constructions manufactured of low-carbon steels. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPOUND OF ELECTRODE COATING | 1992 |
|
RU2056991C1 |
ELECTRODE COATING COMPOSITION | 0 |
|
SU933336A1 |
COMPOSITION OF CHARGE FOR COATING ELECTRODES DESIGNED FOR WELDING LOW CARBON STEEL | 2008 |
|
RU2383418C1 |
WELDING ELECTRODE | 0 |
|
SU1731551A1 |
COMPOSITION OF ELECTRODE COATING FOR WELDING OF LOW-CARBON STEELS | 1994 |
|
RU2070497C1 |
ELECTRODE COATING MATERIAL | 1996 |
|
RU2110384C1 |
ELECTRODE COATING COMPOSITION | 2001 |
|
RU2198774C1 |
ELECTRODE COATING | 0 |
|
SU1754380A1 |
ELECTRODE COATING COMPOSITION | 2001 |
|
RU2220833C2 |
ELECTRODE COATING COMPOSITION | 0 |
|
SU679360A1 |
Authors
Dates
1995-04-30—Published
1994-07-05—Filed