FIELD: building industry. SUBSTANCE: raw mixture has lime, clay and shale ash slag. Clay components has, wt.-%: MgO 1-6; SO3 3.2-6; R2O 2.5-3.5. Ash slag has up to 25% CaO and has the following grainy composition, %: fraction above 40 mm 10; 40-5 mm 25; 5-3 mm 30; 3-0.1 mm 35. Iron-containing component has, wt.-%: MgO 0.1-0.8; SO3 3.3-6.7. Ratio of mixture components, wt. -% : clay component 13.3-18.7; shale ash slag 13.45-20; iron-containing component 0.28-0.33, and lime component - the rest. EFFECT: enhanced quality of raw mixture. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
FEEDSTOCK MIXTURE FOR PRODUCING CEMENT CLINKER | 1997 |
|
RU2101247C1 |
METHOD OF THERMAL PROCESSING ASH-RICH SOLID FUEL | 2008 |
|
RU2368642C1 |
METHOD OF PRODUCING PORTLAND CEMENT | 2020 |
|
RU2742384C1 |
COMPLEX ADDITIVE FOR PORTLAND CEMENT | 2010 |
|
RU2431623C1 |
METHOD FOR BURNING CEMENT CLINKER | 1992 |
|
RU2035425C1 |
METHOD OF PRODUCING CEMENT | 2009 |
|
RU2414439C2 |
CERAMIC MASS TO MANUFACTURE CERAMIC BRICK | 2010 |
|
RU2440317C1 |
METHOD OF PRODUCING CEMENT ON BELITE CLINKER AND SLOW-CURING CEMENT OBTAINED ON ITS BASIS | 2020 |
|
RU2736594C1 |
RAW MIX FOR PREPARING PORTLAND CEMENT CLINKER | 1995 |
|
RU2065845C1 |
RAW MATERIAL MIXTURE FOR PRODUCTION OF PORTLAND CEMENT CLINKER | 1996 |
|
RU2074134C1 |
Authors
Dates
1995-05-20—Published
1992-10-13—Filed