FIELD: manufacture of building materials. SUBSTANCE: raw mixture for manufacture of wood building material contains, mas.%: absolute dry hogged wood 28-45; nepheline cement 24-45; magnesium chloride or iron chloride 12-18; the balance, water. Raw material is prepared by mixing hogged wood with aqueous solution of above indicated chloride with subsequent addition of nepheline cement. Products manufactured from offered raw mixture are characterized by compression strength in 30 min of 3.1-4.9 MPa; in 60 min of 5.1-8.1 MPa; in 24 h of 9.1-16.5 MPa; bending strength of 8.1-12.5 MPa; stability in water 0.91-0.95. EFFECT: higher efficiency. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
RAW MIXTURE FOR MANUFACTURE OF WOOD BUILDING MATERIAL | 1992 |
|
RU2036875C1 |
RAW MIXTURE FOR MANUFACTURE OF WOOD BUILDING MATERIAL | 1992 |
|
RU2036876C1 |
RAW MIXTURE FOR MANUFACTURE OF WOOD BUILDING MATERIAL | 1992 |
|
RU2036874C1 |
MOLDING MATERIAL FOR MANUFACTURE OF WOOD BUILDING MATERIAL | 1991 |
|
RU2036873C1 |
RAW MIXTURE FOR PRODUCTION OF WOOD BUILDING MATERIALS | 1992 |
|
RU2035429C1 |
RAW MATERIAL MIXTURE FOR WOOD BUILDING MATERIALS PRODUCTION | 0 |
|
SU1804454A3 |
RAW MIX FOR MANUFACTURING WOOD BUILDING MATERIAL | 0 |
|
SU1794067A3 |
HYDRAULIC VALVELESS IMPACT DEVICE | 1992 |
|
RU2013541C1 |
RAW MIX FOR PREPARING ARBOLITE AND METHOD OF MANUFACTURE THEREOF | 1998 |
|
RU2153478C1 |
METHOD FOR PRODUCING WOOD CONCRETE | 2019 |
|
RU2746720C2 |