FIELD: production of leather articles. SUBSTANCE: after tanning and dyeing leather fabric is treated within 6-10 h by hydrophobic dispersion having concentration 8-15 g/l and pH 4-8. Mentioned above dispersion contains silicon preparations of siloxane and heterogenic siloxane structure, individual water soluble dyes or their mixture, poly(alkoxy)(acyloxy)silsesquioxanes or polyorgano(acyloxy)silsesquiazanes in mixture with surface active substance, their quantities are 0.5-5, 2-8, 4-8 % respectively of mass of half-finished product. EFFECT: improves efficiency of the method. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR DECORATING OF LEATHER AND FUR HALF-FINISHED PRODUCT | 1991 |
|
RU2036973C1 |
POLY(ALKOXY)(ACYLOXY)SILSESQUIOXANES AS GREASING-HYDROPHOBIZING AGENT FOR FUR AND LEATHER SEMIPRODUCT AND A METHOD OF THEIR PREPARING | 1991 |
|
RU2034867C1 |
METHOD OF PRODUCING HYDROPHOBIC LEATHER | 2009 |
|
RU2404260C1 |
POLYORGANO(STEARINOXY)SYLSESQUIAZANES AS A FATTY-WATER-REPELLENT FOR FUR SEMIFINISHED PRODUCT, AND A METHOD OF ITS SYNTHESIS | 0 |
|
SU1808834A1 |
METHOD OF TREATING FUR HIDES | 0 |
|
SU1234433A1 |
METHOD OF PELT PROCESSING | 2010 |
|
RU2437940C1 |
METHOD OF LEATHER TANNING | 1992 |
|
RU2041957C1 |
METHOD OF SKIN PROCESSING FOR FOOTWEAR UPPER | 0 |
|
SU1574634A1 |
METHOD OF DRESSING FUR SKINS | 0 |
|
SU1227680A1 |
METHOD OF LEATHER MANUFACTURE FROM SWINE RAW | 0 |
|
SU1801985A1 |
Authors
Dates
1995-06-09—Published
1992-02-28—Filed