FIELD: production of leather and fur articles. SUBSTANCE: leather and fur half-finished product is treated by 0.1-1.0 % aqueous emulsion of poly(alkoxy)(acyloxy)silsesquioxane having common formula
where R = CH3,C2H5 Alk = C17H35÷C39H79 n is 1-4. The process is carried out at 35-45 C within 1-2 h. EFFECT: improves quality if desired articles. 2 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| POLY(ALKOXY)(ACYLOXY)SILSESQUIOXANES AS GREASING-HYDROPHOBIZING AGENT FOR FUR AND LEATHER SEMIPRODUCT AND A METHOD OF THEIR PREPARING | 1991 |
|
RU2034867C1 |
| METHOD FOR PROCESSING OF LEATHER FABRIC | 1992 |
|
RU2036974C1 |
| METHOD OF TREATMENT OF LEATHER FABRIC | 1998 |
|
RU2135595C1 |
| METHOD OF DRESSING SKIN TISSUE | 1998 |
|
RU2135594C1 |
| POLYORGANO(STEARINOXY)SYLSESQUIAZANES AS A FATTY-WATER-REPELLENT FOR FUR SEMIFINISHED PRODUCT, AND A METHOD OF ITS SYNTHESIS | 0 |
|
SU1808834A1 |
| METHOD OF DRYING LEATHER AND FUR SEMIPRODUCT | 1991 |
|
RU2031951C1 |
| METHOD OF PRODUCING HYDROPHOBIC LEATHER | 2009 |
|
RU2404260C1 |
| METHOD OF FELL BEAMING | 0 |
|
SU1182080A1 |
| COMPOSITION FOR GREASING ARTICLES OF NATURAL LEATHER | 0 |
|
SU1460078A1 |
| METHOD OF FINISHING FUR PELTS | 0 |
|
SU1461763A1 |
Authors
Dates
1995-06-09—Published
1991-12-27—Filed