FIELD: electrical equipment. SUBSTANCE: copper-based composite material for electrical contacts contains cadmium and chromium to increase its hardness and to reduce material resistivity. Composite material contains, mas. cadmium 0.8-1.0; chromium 0.4-2.0; the balance, copper. Additionally offered material may contain graphite in amount of up to 2.0 mas. EFFECT: higher efficiency. 2 cl
Title | Year | Author | Number |
---|---|---|---|
PRODUCTION OF COPPER-BASED COMPOSITE FOR ELECTRIC CONTACTS | 2014 |
|
RU2567418C1 |
CAKED MATERIAL ON THE BASIS OF SILVER FOR ELECTRICAL CONTACTS | 1991 |
|
RU2026580C1 |
MATERIAL FOR ARC-QUENCHING AND BREAKING ELECTRICAL CONTACTS BASED ON COPPER AND METHOD OF ITS PRODUCTION | 2021 |
|
RU2769344C1 |
METHOD OF MATERIAL MANUFACTURING FOR ARC-QUENCHING AND ELECTRIC BREAK CONTACTS AND MATERIAL | 2013 |
|
RU2522584C1 |
METHOD OF PRODUCING CAST COMPOSITE MATERIAL BASED ON COPPER | 2019 |
|
RU2715513C1 |
SINTERED ELECTRO-CONTACT MATERIAL ON BASE OF COPPER | 2010 |
|
RU2415958C1 |
SINTERED ELECTROCONTACT MATERIAL ON THE BASE OF COPPER | 1993 |
|
RU2073736C1 |
HIGH-DUTY CAST IRON | 0 |
|
SU1742348A1 |
CAST ALLOY BASED ON ALUMINIUM TO PRODUCE BY IMPREGNATION OF COMPOSITE MATERIALS WITH CARBON-GRAPHITE FRAMEWORK | 2014 |
|
RU2555737C1 |
METHOD OF PRODUCTION AND TREATMENT OF ALLOYED CASTING MATERIAL, CASTING MATERIAL FOR WORKING PART OF ROLLS AND COMBINED ROLL | 2000 |
|