FIELD: concentration of mineral resources. SUBSTANCE: compound for flotation of sulfide ores contains butyl xanthate and nitrogen sulfide concentrate of oil obtained by twp-stage extraction of its fraction at a boiling point within 200 to 350 C by a solution of zinc chloride in dimethyl ormamide. Relation of components, mass percent: butyl xanthate 33 to 35, nitrogen sulfide concentrate of oil 50 to 67. EFFECT: facilitated procedure of flotation. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF SULFIDE COPPER-NICKEL ORE FLOTATION | 1994 |
|
RU2067030C1 |
METHOD OF SULFIDE COPPER-NICKEL ORES FLOTATION | 1992 |
|
RU2071837C1 |
COPPER-NICKEL SULFIDE FLOTATION PROCESS | 1997 |
|
RU2131303C1 |
METHOD FOR FLOTATION OF SULFIDE COPPER-NICKEL ORES | 1995 |
|
RU2097141C1 |
METHOD FOR FLOTATION OF SULFIDE COPPER-NICKEL ORES | 1994 |
|
RU2067029C1 |
METHOD OF EXTRACTION OF SULFIDES FROM TUNGSTEN-CONTAINING ORES | 1991 |
|
RU2034068C1 |
METHOD FOR REMOVING SULFIDES OF TUNGSTEN-CONTAINING ORES | 1991 |
|
RU2031732C1 |
METHOD FOR REMOVING SULFIDES OF TUNGSTEN-CONTAINING ORES | 1991 |
|
RU2031731C1 |
METHOD OF FLOTATION OF THE POLYMETALLIC GOLD-CARRYING ORES | 2005 |
|
RU2280509C1 |
METHOD FOR BULK FLOTATION OF POLYMETALLIC ORES BASED ON USE OF MICROEMULSIONS | 2023 |
|
RU2821082C1 |
Authors
Dates
1995-07-09—Published
1992-02-24—Filed