FIELD: concentration of mineral resources. SUBSTANCE: bulk flotation is conducted in alkaline medium produced by lime with introduction of copper-molybdenum concentrate. The latter is treated by oxygen at a temperature of 60 to 95 C. Selective flotation of copper-molybdenum concentrate is conducted with separation of molybdenum to a froth product. Acidifying thermal treatment is accomplished at a pressure of 0.05 to 1.0 MPa, beginning at pH-value within 11.0 to 8.5 and completing at pH-value within 8.0 to 6.0. Selective flotation is conducted at pH-value within 6.0 to 8.0. EFFECT: facilitated procedure. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF COPPER-MOLYBDENUM ORES SEPARATION | 2012 |
|
RU2481410C1 |
METHOD OF SELECTIVE FLOTATION OF SULFIDE COPPER-ZINC ORES | 1992 |
|
RU2038860C1 |
METHOD FOR FLOTATION OF SULFIDE COPPER/ZINC ORES | 1993 |
|
RU2042433C1 |
METHOD FOR FLOATING SEPARATION OF COLLECTIVE SULFIDE COPPER/ZINK CONCENTRATE | 1991 |
|
RU2042431C1 |
METHOD FOR FLOTATION TREATMENT OF FLOWING AND AGED MINE REFUSES CONTAINING COPPER AND MOLYBDENUM MINERALS | 2013 |
|
RU2539448C1 |
FLOTATION METHOD | 1981 |
|
SU1010759A1 |
METHOD OF FLOTATION OF COPPER-MOLYBDENUM ORE | 2007 |
|
RU2340405C1 |
METHOD OF FLOTATION OF COPPER MOLYBDENUM ORES | 2007 |
|
RU2340406C1 |
METHOD FOR FLOTATION OF SULFIDE ZINC BEARING ORES | 1992 |
|
RU2034664C1 |
METHOD OF DRESSING OF OXIDIZED COPPER ORES | 1992 |
|
RU2012416C1 |
Authors
Dates
1995-07-09—Published
1990-03-05—Filed