FIELD: manufacture of building materials. SUBSTANCE: raw mixture includes, mas. cement 76.56-76.835; lignosulfonate successively treated with 33% aqueous solution of hydrogen peroxide in ratio of 19:1 and 14% aqueous solution of nitric acid in ratio of 7:1 0.115-0.46, the balance, water. Additive improves rheological properties of mixture without impairing its strength. Mobility of mixture is up to 14.8 cm and strength after 28 days of hardening under normal conditions is up to 61.05 MPa. EFFECT: higher efficiency. 9 tbl
Title | Year | Author | Number |
---|---|---|---|
RAW MATERIALS MIXTURE | 1992 |
|
RU2015947C1 |
METHOD OF PRODUCING ADDITION FOR CONCRETE MIXTURE | 1997 |
|
RU2133239C1 |
METHOD OF PREPARING PLASTICIZING ADDITIVE | 1997 |
|
RU2125028C1 |
CONCRETE MIX | 1997 |
|
RU2133238C1 |
BINDER | 2002 |
|
RU2237032C2 |
RAW MEAL | 2000 |
|
RU2199497C2 |
BINDER | 1993 |
|
RU2076120C1 |
BINDER | 0 |
|
SU1754685A1 |
PLASTICISING AND WATER-REDUCING ADDITIVE FOR CONCRETE AND MORTAR | 2011 |
|
RU2476396C1 |
INITIAL COMPOSITION FOR PRODUCING ASBESTOS-CONCRETE ARTICLES | 0 |
|
SU1618739A1 |
Authors
Dates
1995-07-20—Published
1992-05-15—Filed