FIELD: preparation of vibroabsorbing mastic. SUBSTANCE: the process comprises successively mixing the following components (wt): 40.3-49.7 polyvinyl acetate epoxy dispersion comprising 51-57 wt dry matter with 1.0-4.7 alkylbenzylpyridinium chloride such as 4.5-12.6 chalk, 14.0-32.6 vermiculite, 13.0-18.7 fire- proofing nepheline compound and 0.5-5.0 epoxy resin hardener. Fillers and fire proofing compound may be added in any sequence but after the addition of alkylbenzylpyridinium chloride. EFFECT: improved properties of the mastic. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
VIBRATION-ABSORBING MASTICS | 1991 |
|
RU2044018C1 |
VIBRATION ABSORBING PASTE | 2009 |
|
RU2408637C1 |
METHOD OF SYNTHESIS OF VIBRATION-ABSORBING MASTIC | 1991 |
|
RU2044016C1 |
VIBRATION-ABSORBING MASTICS | 1991 |
|
RU2044017C1 |
VIBRO-ABSORBING MASTIC AND METHOD OF PREPARATION THEREOF | 2000 |
|
RU2186814C2 |
VIBRATION-ABSORBING MASTIC | 1991 |
|
RU2035482C1 |
VIBRATION ABSORBING PASTE | 2009 |
|
RU2405016C1 |
VIBRATION-ABSORBING PASTE | 2007 |
|
RU2375398C2 |
VIBRATION ABSORBING PASTE | 2012 |
|
RU2522345C1 |
VIBRATION-ABSORBING EPOXIDE COMPOSITION | 2012 |
|
RU2507228C1 |
Authors
Dates
1995-07-20—Published
1991-11-26—Filed