FIELD: decorative coating applying. SUBSTANCE: for preparing golden surface article is treated by immersing in the bath with solution consisting of six parts varnish and four parts turpentine or white spirit at 25-30 C followed by drying and thermal treatment by roasting at temperature above 150 C for 10-15 min. EFFECT: improved method of applying. 2 cl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MAKING ARTISTIC GOODS FROM WOOD WITH "KHOKHLOMA" PAINTING | 0 |
|
SU1831446A3 |
METHOD FOR ARTICLE SURFACE DECORATIVE MODIFICATION | 1993 |
|
RU2015032C1 |
METHOD FOR MANUFACTURE OF DECORATIVE ARTISTIC ARTICLES WITH "KHOKHLOMA" ORNAMENT | 2002 |
|
RU2240236C2 |
METHOD OF DECORATION OF ARTISTIC PRODUCTS WITH IMITATION OF GILDING | 1998 |
|
RU2140362C1 |
METHOD FOR MANUFACTURE OF ICON WITH SIMULATION OF GILDING | 2001 |
|
RU2211763C2 |
METHOD TO MAKE ART OBJECTS OF WOOD WITH KHOKHLOMA ORNAMENT | 2010 |
|
RU2415030C1 |
METHOD OF MAKING DECORATIVE NATURAL STONE-IMITATING COATING ON WOOD SURFACE | 2011 |
|
RU2459712C1 |
METHOD FOR ARTISTIC-DECORATIVE MODIFICATION OF ARTICLE SURFACES | 2000 |
|
RU2179931C1 |
METHOD OF ARTISTIC-DECORATIVE MODIFICATION OF ARTICLE SURFACES | 1996 |
|
RU2111126C1 |
METHOD TO MANUFACTURE DECORATIVE ART OBJECTS WITH ZHOSTOV ORNAMENT | 2010 |
|
RU2411134C1 |
Authors
Dates
1995-08-20—Published
1993-12-14—Filed