FIELD: recovery of mineral acids from solutions. SUBSTANCE: 30.3-35.6 wt 2-methyl-5-vinylpyridine, 3.0- 3.6 wt divinyl benzene and 0.6-0.8 wt benzoyl peroxide are polymerized in the presence of 60-66 wt fluoroplastic-26. The resulting product is homogenized and dispersed in an organic solvent and a film is moulded from this organic dispersion. EFFECT: improved recovery process. 1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD OF PLASTIC GRANULATOR PRODUCING | 1996 |
|
RU2096341C1 |
| PROCESS FOR PREPARING SOLID BIOSORBENTS FOR RECOVERY OF METALS | 1992 |
|
RU2045574C1 |
| METHOD OF PREPARING OF BIOCATALYST FOR GLUCOSE ISOMERIZATION | 1990 |
|
RU2031124C1 |
| THERMOPLASTIC POLYMER MATERIAL | 1996 |
|
RU2115672C1 |
| METHOD OF IMMOBILIZED UREAS PREPARING | 1990 |
|
RU2031120C1 |
| METHOD OF TRIS-β-CHLOROPROPYLPHOSPHATE PURIFICATION | 1992 |
|
RU2037497C1 |
| METHOD OF PREPARING MODIFIED SORBENT | 1996 |
|
RU2105015C1 |
| METHOD OF PRODUCING THE POLYHALOID ANION-EXCHANGE RESIN | 1995 |
|
RU2083604C1 |
| METHOD FOR MANUFACTURE OF POLYMERIC MEMBRANES | 1992 |
|
RU2026726C1 |
| POLYMER PIEZOELECTRIC MATERIAL | 1993 |
|
RU2036182C1 |
Authors
Dates
1995-08-20—Published
1991-06-26—Filed