FIELD: polymer piezoelectric materials. SUBSTANCE: proposed material contains (mass parts): ceramic powder of lead titanate which contains additive of 0.01-5 mass % manganese oxide 400-1200, organic polymer matrix 100, plasticizer 10-30 and cross-linking agent 2.5-16. Polybutadiene chloride, polyvinylchloride or their mixture are used as mentioned above organic polymer matrix. Mixture of zinc oxide, magnesium oxide and stearic acid at ratio 1: 1: 0.5-7: 7.2-2.5-16 is used as mentioned above cross-linking agent. Thus prepared material has high elasticity and may be processed by extrusion. EFFECT: improves quality of the material. 4 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
ELECTROCONDUCTIVE POLYMERIC COMPOSITION | 1992 |
|
RU2016424C1 |
METHOD OF PLASTIC GRANULATOR PRODUCING | 1996 |
|
RU2096341C1 |
THERMAL PLASTIC COMPOSITION | 1995 |
|
RU2076121C1 |
PRESS-COMPOSITION | 1992 |
|
RU2034876C1 |
THERMOPLASTIC POLYMER MATERIAL | 1996 |
|
RU2115672C1 |
METHOD OF TRIS-β-CHLOROPROPYLPHOSPHATE PURIFICATION | 1992 |
|
RU2037497C1 |
ANTIFRICTION COMPOSITION | 1992 |
|
RU2016002C1 |
MULTIFUNCTIONAL POLYMER COMPOSITE -VARIOCOMPOSITE- AND METHOD OF MANUFACTURE THEREOF | 1993 |
|
RU2114740C1 |
HEAT RESISTANT ADHESIVE COMPOSITION | 1992 |
|
RU2061727C1 |
THERMOPLASTIC POLYMER COMPOSITION | 1992 |
|
RU2057152C1 |
Authors
Dates
1995-05-27—Published
1993-03-10—Filed