FIELD: chemical technology. SUBSTANCE: method involves sulfuric acid decomposition of boron-containing raw, leaching chamber product with reusable solutions, A2B3 extraction from debalanced solutions by their treatment with calcined waste of datolite ore concentration or calcined limestone up to pH 10-12, washing slime with mother liquids of calcium borate, acidification of production liquid after leaching, crystallization of boric acid, drying, package. EFFECT: increased yield of product, simplified technology, decreased exhaust to environment. 2 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD OF BORIC ACID PRODUCTION | 1986 |
|
RU1471482C |
| METHOD OF OBTAINING BORIC ACID | 1982 |
|
RU1075583C |
| METHOD OF BORIC ACID PRODUCING | 1987 |
|
RU1504959C |
| METHOD OF OBTAINING BORIC ACID | 1982 |
|
SU1135124A1 |
| DATOLITE ORE CONCENTRATION METHOD | 1992 |
|
RU2053027C1 |
| BORIC ORES FLOTATION METHOD | 1993 |
|
RU2057595C1 |
| METHOD OF BORIC ACID PRODUCING | 1988 |
|
RU1601938C |
| METHOD FOR COMPACTION OF BOROSILICATE POWDERS | 1992 |
|
RU2015846C1 |
| METHOD OF CALCIUM BORATE PRODUCING | 1988 |
|
RU1584313C |
| METHOD OF PRODUCING CALCIUM BORATE | 0 |
|
SU859294A1 |
Authors
Dates
1995-10-10—Published
1992-08-19—Filed