FIELD: metallurgy. SUBSTANCE: method includes addition of 1.5-3.5% of ammonium sulfate to boric acid used as binding agent. This procedure allows increase of degree of transition of boron into carbon-soluble form from 86 to 95-98% that facilitates increase of final product yield. Besides, grinding of briquettes after calcination in drum-type furnace is easier. EFFECT: higher efficiency. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF BOROSILICATE POWDER COMPACTING | 0 |
|
SU1771882A1 |
METHOD OF CATALYST MAKING FOR OIL FRACTION HYDROREFINING | 1992 |
|
RU2008972C1 |
METHOD OF MANUFACTURING CERAMICS WITH LOW DIELECTRIC PERMITTIVITY | 1994 |
|
RU2083529C1 |
METHOD OF PROCESSING BOROSILICATE CONCENTRATES | 2008 |
|
RU2375305C1 |
METHOD FOR SOLIDIFYING TRANSURANIUM FUEL ELEMENT SOLUTIONS | 1994 |
|
RU2095867C1 |
METHOD OF IRRADIATED BORON CARBIDE PROCESSING | 1999 |
|
RU2156732C1 |
METHOD FOR DYNAMIC TREATMENT OF POWDER MATERIALS | 2000 |
|
RU2192333C2 |
PERICLASE-SPINEL REFRACTORY | 1998 |
|
RU2124487C1 |
METHOD OF PRODUCTION OF REDUCED MATERIALS FROM ORE STOCK | 1995 |
|
RU2096482C1 |
CHARGE FOR CERAMIC MATERIAL PRODUCTION | 2007 |
|
RU2353600C2 |
Authors
Dates
1994-07-15—Published
1992-06-23—Filed