FIELD: production of consumer goods. SUBSTANCE: method for production of polymer, composition includes mixing with heating of PVC, thermal stabilizer, plasticizer and lubricant. Lubricant is preliminarily mixed with plasticizer at 60-80 C for 20-30 min, and obtained mixture is mixed with PVC and thermal stabilizer and heated up to 100-110 C. Mass fraction of soluble matter from polymer materials amounts to 0.25- 0.33, odor and taste of aqueous extract is 1 point. Static thermostability of polymer composition is 150-235 min, dynamic thermostability is 80-155 min. EFFECT: higher efficiency. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
0 |
|
SU1781251A1 | |
POLYMERIC COMPOSITION | 1992 |
|
RU2048493C1 |
POLYMERIC COMPOSITION | 1992 |
|
RU2048492C1 |
ANAEROBIC HERMETIC COMPOSITION | 1991 |
|
RU2036947C1 |
POLYMER COMPOSITION | 0 |
|
SU1758047A1 |
POLYMERIC COMPOSITION | 1993 |
|
RU2088612C1 |
METHOD OF POLYMERIC COMPOSITION PREPARING | 1990 |
|
SU1702676A1 |
POLYMERIC COMPOSITION | 1992 |
|
RU2048496C1 |
POLYMERIC COMPOSITION | 1993 |
|
RU2086584C1 |
METHOD OF PREPARING FILLED POLYMERIC COMPOSITION | 1989 |
|
SU1755558A1 |
Authors
Dates
1995-10-10—Published
1992-04-23—Filed