FIELD: for packing and containers having improved whiteness. SUBSTANCE: the polymeric composition comprises (wt parts): 100 PVC; 1-3 thermostabilizer and 4-25 grafted copolymer; 2-60 wt vinyl chloride per 40-98 wt rubber elastomer containing links (wt ): 67-74 butadiene and 26-33 styrene. The stretch ratio is 1:2 (1:2.8), the whiteness variation degree after ageing in a weatherometer for 1500 hrs is 0.70-0.72. EFFECT: improved properties of the polymeric composition. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
POLYMERIC COMPOSITION | 1993 |
|
RU2086584C1 |
METHOD FOR PRODUCING GRAFT COPOLYMER OF VINILCHLORIDE | 1992 |
|
RU2070209C1 |
POLYMER COMPOSITION | 1992 |
|
RU2045552C1 |
METHOD FOR PRODUCTION OF MODIFYING AGENT FOR POLYVINYL CHLORIDE | 1992 |
|
RU2074202C1 |
POLYMER COMPOSITION | 1992 |
|
RU2045551C1 |
PROCESS FOR PREPARING MODIFIED POLYVINYL CHLORIDE | 1994 |
|
RU2084461C1 |
POLYMERIC COMPOSITION | 1992 |
|
RU2048495C1 |
POLYMERIC COMPOSITION | 1994 |
|
RU2084473C1 |
POLYMER COMPOSITION | 1992 |
|
RU2076119C1 |
PROCESS FOR PREPARING GRAFTED COPOLYMER OF VINYL CHLORIDE WITH ETHYLENE-VINYL ACETATE COPOLYMER | 1993 |
|
RU2082724C1 |
Authors
Dates
1995-11-20—Published
1992-05-26—Filed