FIELD: alkali chemical power supplies. SUBSTANCE: device has housing with electrolyte, which is heavy-water solution of alkali, porous positive nickel oxide electrode unit and porous negative iron electrode unit. Capacity of first electrode unit is 1.2-2.0 of capacity of second one. In addition device has porous separators, which size is less than size of electrode pores. EFFECT: decreased gas emission, improved specific electric characteristics. 2 cl
Title | Year | Author | Number |
---|---|---|---|
ALKALI IRON-NICKEL ACCUMULATOR AND METHOD FOR ITS USE | 1993 |
|
RU2056677C1 |
SECONDARY LOW-GAS-EMISSION CHEMICAL POWER SUPPLY | 2000 |
|
RU2168808C1 |
NICKEL-IRON STORAGE CELL | 1995 |
|
RU2098895C1 |
ELECTROLYTE FOR CHEMICAL SOURCE OF ELECTRIC ENERGY | 1993 |
|
RU2054759C1 |
NICKEL-ZINC STORAGE CELL | 1994 |
|
RU2069924C1 |
SEALED ALKALINE CELL | 1996 |
|
RU2112301C1 |
METHOD FOR PRODUCING SEALED ALKALINE CELL WITH NICKEL-OXIDE POSITIVE AND CADMIUM NEGATIVE PLATES | 2004 |
|
RU2280298C2 |
NICKEL-CADMIUM CELL | 1995 |
|
RU2099820C1 |
HERMETICALLY SEALED NICKEL-CADMIUM ACCUMULATOR | 1999 |
|
RU2168810C2 |
METHOD TO OPERATE ELECTROCHEMICAL CAPACITORS | 2012 |
|
RU2520183C2 |
Authors
Dates
1996-03-20—Published
1994-04-12—Filed