FIELD: obtaining of rhenic sulfide concentrate. SUBSTANCE: method involves depositing rhenium together with osmium, with sulfuric acid concentration being maintained within 15-30%, solution temperature being 80-107 C and consumption of sodium thiosulfate 5-15 g/dm3. EFFECT: increased efficiency and improved quality of concentrate. 1 tbl