FIELD: production of ceramic pigment. SUBSTANCE: proposed mixture contains (mass %): calcium oxide 813, cobalt oxide 3-6, titanium oxide 43-46, magnesium 10-11.5, calcium sulfate 30-35. Temperature of heat treatment of desired pigment is 730-750 C, its covering power being 59 g/m2. EFFECT: improves quality of desired product. 1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| MIXTURE FOR PRODUCTION OF CERAMIC PIGMENT | 1992 |
|
RU2057728C1 |
| CHARGE FOR CERAMIC PIGMENT | 1992 |
|
RU2029745C1 |
| DAUBING FOR PROTECTION OF METALLIC SURFACES | 1991 |
|
RU2057739C1 |
| METHOD OF PRODUCING CERAMIC PIGMENTS OF SPINEL TYPE | 2015 |
|
RU2580542C1 |
| METHOD OF PRODUCTION OF CORDIERITE | 1992 |
|
RU2062771C1 |
| UNDERGLAZE BLUE DYE | 1997 |
|
RU2148556C1 |
| CHARGE FOR MOLDED CERAMIC ARTICLE MAKING | 1991 |
|
RU2028281C1 |
| CATALYST FOR PROFOUND HYDROCARBON OXIDATION | 1992 |
|
RU2043145C1 |
| CERAMIC OVERGLAZED DYE | 1992 |
|
RU2033981C1 |
| MORTAR FOR LINING HIGH TEMPERATURE UNITS | 1992 |
|
RU2065426C1 |
Authors
Dates
1996-04-10—Published
1992-04-07—Filed