FIELD: production of thermoplastic compositions. SUBSTANCE: desired composition contains 40-75 mass % of vinyl aromatic polymer. Said polymer contains 5-15 mass % of polybutadiene rubber and 0.5-5 mass % of block copolymer. Said block copolymer contains (mass %): styrene 25-75, butadiene 75-25, polyethylene 5-50 and grafted styrene ethylene diene rubber 10-50. Said grafted styrene ethylene diene rubber contains 2-20 mass % of diene. EFFECT: improves quality of desired product. 6 tbl
Authors
Dates
1996-06-10—Published
1991-11-11—Filed