FIELD: glass coatings. SUBSTANCE: nonperspirating coating is prepared from 5% aqueous solution of iron-containing polyacrylic acid. Coating is applied on glass surface and dried at constant temperature. Time for film protecting effect is 770-15000 s. EFFECT: enhanced quality of coating.
Title | Year | Author | Number |
---|---|---|---|
INSTALLATION FOR PRODUCING IRON-CONTAINING POLYACRYLIC ACID | 1996 |
|
RU2112593C1 |
COMPOSITION FOR COATING FRUITS AND VEGETABLES | 0 |
|
SU1375221A1 |
METHOD FOR ISOLATION OF VANlLLIN | 1993 |
|
RU2078754C1 |
METHOD FOR SORPTION OF HEAVY METALS OF AQUEOUS SOLUTIONS | 1996 |
|
RU2101370C1 |
COPOLYMER OF ACRYLIC ACID WITH EPICHLORHYDRIN AS WATER-SOLUBLE TECHNOLOGICAL GLUE | 1994 |
|
RU2068853C1 |
PROCESS FOR PREPARING AROMATIC OXYALDEHYDES | 1992 |
|
RU2057112C1 |
PREPARATION FOR COMPLEX PROTECTION OF METALS FROM CORROSION, BIOFOULING AND SCALE | 1996 |
|
RU2109847C1 |
CROSS-LINKED CO-CONTAINING POLYACRYLIC ACID AS A SUPERSORBENT | 1993 |
|
RU2074200C1 |
STYRENE COPOLYMERS WITH FLUORO-CONTAINING VINYLTHIOBENZENE DERIVATIVES AS HEAT-RESISTANT AND HIGH-STRENGTH MATERIALS | 1992 |
|
RU2005728C1 |
PROCESS FOR PREPARING 2,2,-BIS-(3,5-DIBROMO-4- HYDROBYPHENYL) PROPANE | 1992 |
|
RU2034823C1 |
Authors
Dates
1996-06-27—Published
1993-04-14—Filed